The laser plastic welding design & development guide for engineers

Our Laser Plastic Welding Design & Development Guide is a free, 63-page reference for engineers taking a welded plastic part from concept to production. It covers wavelengths, material pairs, joint geometry, clamping and the project roadmap we use with every customer.
It is written by the engineers who run our weld trials, and it is built from the same slides we walk customers through before their first sample run.
Why we wrote this guide
Most laser plastic welding projects that fail do so before a laser ever fires. The wrong material pair, a joint with no room for melt collapse, or a part that cannot be clamped flat will sink a project no matter how good the equipment is.
We wanted one document that answers the questions we get on every first call, so your design reaches the lab ready to weld. Use it to avoid failures, choose the right process, and launch on time.
Wavelengths: 1µm v. 2µm
The two most common process wavelengths behave very differently. At 1µm, the laser passes through a transparent upper part and is absorbed at the surface of an absorbing lower part, usually one loaded with carbon black or an IR additive. At 2µm, the plastic itself absorbs the energy through its thickness, so clear-to-clear welds are possible without additives.
The guide also covers specialty wavelengths like 1.7µm, which absorbs near the surface, and explains which job each wavelength fits.
Material combinations
Not every pair of plastics will weld. Compatible melt temperatures, overlapping processing windows and chemical compatibility all matter, and colorants, glass fill and other additives can change the result entirely.
- Amorphous v. semi-crystalline polymers, and why it matters for transmission
- How colorants and IR absorbers set the weld interface at 1µm
- Melt overlap and chemical compatibility between dissimilar plastics
Part and joint design
Joint design decides whether a weld is strong, sealed and repeatable. The guide gives best practices for parts of every size, from simple lap joints to collapse ribs and radial joints, with separate rules for each wavelength.
Clamping, the part most guides skip
Clamping is arguably the most important aspect of laser plastic welding. Without consistent contact at the joint, the melt cannot bridge the gap. The guide covers the tools available to you, proper clamp forces, and how to hold tolerances for solid joint contact:
- Glass and acrylic clamp tools
- Metal outer and hybrid clamp tools
- Radial weld mirror tools
- Clamp force and joint contact
I’ve dedicated 15 years to one mission: pushing the boundaries of laser-based manufacturing. Dax Hamilton, Founder, Dax Research
Inside the guide
The guide runs eight modules across 63 pages:
| Module | What it covers |
|---|---|
| 01. Development roadmap | The three phases of a successful project, and the project data you need up front. |
| 02. Why laser plastic welding? | Advantages, disadvantages, and where strong, clean, particulate-free bonds matter. |
| 03. Choosing the right wavelength | 1µm, 2µm and 1.7µm compared, and which laser fits which job. |
| 04. Process types and optics | Contour, simultaneous and scanner welding; Gaussian v. flat-top beams. |
| 05. Material compatibility | Amorphous v. semi-crystalline, melt overlap and chemical compatibility. |
| 06. 1µm design guidelines | Transmission, absorption and colorants; lap joints, collapse ribs, radial joints. |
| 07. 2µm design guidelines | Bulk absorption in clear parts, pseudo-ribs and T welds. |
| 08. 1.7µm design guidelines | Near-surface absorption and general guidelines for 1.7µm. |
Ready to make your concept a reality? Download the guide below, or talk to our engineers about your part.
Get the full guide
The full 63-page guide, sent straight to your inbox. No sales call required.